Statement: In the blast furnace, limestone calcination occurs in the stack at approximately 800–900°C; the CaO produced reacts with silica gangue to form calcium silicate (CaSiO₃) slag, with target basicity CaO/SiO₂ ≈ 1.0–1.2.